In an EDM process using an RC relaxation circuit, a 12 mm diameter through hole is made in a steel plate of 50 mm thickness using a graphite tool and kerosene as the dielectric. machining is carried out under the following conditions:

Resistance = 40 Ω 

Capacitance = 20 μF

Supply Voltage = 220 V

Discharge voltage = 110 V

Find the time for one cycle in milliseconds.

Enter numerical value using the virtual keypad. Round off where necessary.