Match the casting defects (Group A) with the probable causes (Group B) :

Group A

Group B

P: Hot tears

1: Improper fusion of two streams of liquid metal

Q: Shrinkage

2: Low permeability of the sand mould

R: Blow holes

3: Volumetric contraction both in liquid and solid stage

S: Cold shut

4: Differential cooling rate

1
P – 1, Q – 3, R – 2, S – 4
2
P – 4, Q – 3, R – 2, S – 1
3
P – 3, Q – 4, R – 2, S – 1
4
P – 1, Q – 2, R – 4, S – 3